ATOM ARC 8018-B3L

Atom Arc 8018-B3L is an all-position low hydrogen electrode designed for welding the nominal 2% Cr - 1% Mo steels. The low carbon analysis of the weld metal contributes to its crack resistance, and the careful blend of Cr/Mo provide the properties needed for weldments subjected to elevated temperature service.

Ordering Information
SKU255173114
UPC662303018320
Model / Product DescriptionAA 8018-B3L 3/16X14X50#HS
Item Weight50.00
Min Order50
Filler Metal Spec Def 
Size3/16 , 14
Length14 in., 50 in.
Weight50 lbs., Hermetically Sealed Can lbs.
PackageHermetically Sealed Can