ATOM ARC 9018-CM

Atom Arc 9018-CM is an all-position low hydrogen electrode designed for welding 2.5% Cr - 1% Mo steels commonly used in pressure vessels, heat exchangers and related components.

Ordering Information
SKU255071466
UPC662303081447
Model / Product DescriptionAA 9018-CM 3/16X14X50#HS XF
Item Weight50.00
Min Order50
Filler Metal Spec Def 
Size3/16
Length14 in.
Weight50 lbs.
PackageHermetically Sealed Can