Atom Arc 9018-CM is an all-position low hydrogen electrode designed for welding 2.5% Cr - 1% Mo steels commonly used in pressure vessels, heat exchangers and related components.
| SKU | 255071813 |
|---|---|
| UPC | 662303017439 |
| Model / Product Description | AA 9018-CM 1/8X14X50#HS |
| Item Weight | 50.00 |
| Min Order | 50 |
| Filler Metal Spec Def | |
| Size | 1/8 , 14 |
| Length | 14 in., 50 in. |
| Weight | 50 lbs., Hermetically Sealed Can lbs. |
| Package | Hermetically Sealed Can |
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.