Atom Arc 7018-C3L

Atom Arc 7018-C3L is a low hydrogen, iron powder electrode that produces a low carbon 1% nickel weld metal deposit.

Ordering Information
SKU255028953
UPC662303048174
Model / Product DescriptionAA 7018-C3L 5/32X14X50#HS
Item Weight50.00
Min Order50
Filler Metal Spec Def 
Size5/32 , 14
Length14 in., 50 in.
Weight50 lbs., Hermetically Sealed Can lbs.
PackageHermetically Sealed Can