ATOM ARC 8018

Atom Arc 8018 electrodes deposit 1% Ni weld metal. It is used primarily to weld high-tensile steels, especially where notch toughness at low temperatures is required.

Ordering Information
SKU255047318
UPC662303017149
Model / Product DescriptionAA 8018 7/32X18X50#HS
Item Weight50.00
Min Order50
Filler Metal Spec Def 
Size7/32 , 18
Length18 in., 50 in.
Weight50 lbs., Hermetically Sealed Can lbs.
PackageHermetically Sealed Can