Atom Arc 8018-N is an all-position low hydrogen electrode that deposits weld metal with 3% Ni content. This electrode is used when low temperature notch toughness values are required.
| SKU | 255033326 |
|---|---|
| UPC | 662303016982 |
| Model / Product Description | AA 8018-N 3/32X14X10#HS |
| Item Weight | 10.00 |
| Min Order | 10 |
| Filler Metal Spec Def | |
| Size | 3/32 , 14 |
| Length | 14 in., 10 in. |
| Weight | 10 lbs., Hermetically Sealed Can lbs. |
| Package | Hermetically Sealed Can |
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.