ATOM ARC 9018

Atom Arc 9018 is an all-position low hydrogen electrode designed for use on high-tensile quenched and tempered steels.

Ordering Information
SKU255061806
UPC662303017323
Model / Product DescriptionAA 9018 3/32X14X50#HS
Item Weight50.00
Min Order50
Filler Metal Spec Def 
Size3/32 , 14
Length14 in., 50 in.
Weight50 lbs., Hermetically Sealed Can lbs.
PackageHermetically Sealed Can