Print this page

ATOM ARC 9018

Atom Arc 9018 is an all-position low hydrogen electrode designed for use on high-tensile quenched and tempered steels.

Ordering Information
SKU255061814-03
UPC662303060206
Model / Product DescriptionAA 9018 1/8X14X50#HS
Item Weight50.00
Min Order50
Filler Metal Spec Def 
Size1/8
Length14 in.
Weight50 lbs.
PackageHermetically Sealed Can