ATOM ARC 10018

Atom Arc 10018 is an all-position low hydrogen electrode used primarily for applications requiring weld joints of at least 100 ksi (690 MPa) tensile strength, good ductility and crack resistance.

Ordering Information
SKU255081416
UPC662303017538
Model / Product DescriptionAA 10018 1/4X18X50#HS
Item Weight50.00
Min Order50
Filler Metal Spec Def 
Size1/4 , 18
Length18 in., 50 in.
Weight50 lbs., Hermetically Sealed Can lbs.
PackageHermetically Sealed Can