Atom Arc 7018-AC is an all-position low hydrogen electrode specifically designed to have optimum arc characteristics when used with AC power sources. It offers easy arc starting, smooth arc and low spatter.
| SKU | 255028599 |
|---|---|
| UPC | 662303016630 |
| Model / Product Description | AA 7018-AC 5/32X14X10#HS |
| Item Weight | 10.00 |
| Min Order | 10 |
| Filler Metal Spec Def | |
| Size | 5/32 , 14 |
| Length | 14 in., 10 in. |
| Weight | 10 lbs., Hermetically Sealed Can lbs. |
| Package | Hermetically Sealed Can |