Print this page

ATOM ARC 7018-AC

Atom Arc 7018-AC is an all-position low hydrogen electrode specifically designed to have optimum arc characteristics when used with AC power sources. It offers easy arc starting, smooth arc and low spatter.

Ordering Information
SKU255028672
UPC662303029180
Model / Product DescriptionAA 7018-AC 5/32X14X10#VALP
Item Weight10.00
Min Order10
Filler Metal Spec Def 
Size5/32 , 14
Length14 in., 10 in.
Weight10 lbs., Value Pack lbs.
PackageValue Pack

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.