Atom Arc 7018-M is an E7018M all-position low hydrogen electrode specially formulated to meet the more stringent requirements of Military Specification MIL-E-0022200/10.
| SKU | 255014128 |
|---|---|
| UPC | 662303016319 |
| Model / Product Description | AA 7018-M 5/32X14X10#HS |
| Item Weight | 10.00 |
| Min Order | 10 |
| Filler Metal Spec Def | |
| Size | 5/32 , 14 |
| Length | 14 in., 10 in. |
| Weight | 10 lbs., Hermetically Sealed Can lbs. |
| Package | Hermetically Sealed Can |