ATOM ARC 7018-M

Atom Arc 7018-M is an E7018M all-position low hydrogen electrode specially formulated to meet the more stringent requirements of Military Specification MIL-E-0022200/10.

Ordering Information
SKU255014151
UPC662303067946
Model / Product DescriptionAA 7018-M 1/4X18X10#HS
Item Weight10.00
Min Order10
Filler Metal Spec Def 
Size1/4
Length18 in.
Weight10 lbs.
PackageHermetically Sealed Can