Print this page

ARCALOY 308L-16

Arcaloy 308L-16 was developed for welding 304L stainless.

Ordering Information
SKU251013306
UPC662303013011
Model / Product DescriptionAC 308L-16 3/32X9X6#HS SPECIAL ORDER ONLY
Item Weight6.00
Min Order6
Filler Metal Spec Def 
Size9 , 3/32
Length6 in., 9 in.
WeightHermetically Sealed Can lbs., 6 lbs.
PackageHermetically Sealed Can