ARCALOY 308/308H-16

Arcaloy 308/308H-16 was developed for welding types 304H and 347H stainless when high temperature service is required.

Ordering Information
SKU252026620
UPC662303014995
Model / Product DescriptionAC 308/308H-16 1/4X14X10#HS
Item Weight10.00
Min Order10
Filler Metal Spec Def 
Size1/4 , 14
Length14 in., 10 in.
Weight10 lbs., Hermetically Sealed Can lbs.
PackageHermetically Sealed Can