Print this page

ARCALOY 309L-15

Arcaloy 309L-15 is used primarily in the overlay of steel or to join stainless steel to carbon or low alloy steels. Best used out-of-position on DC current only.

Ordering Information
SKU251063103
UPC662303013479
Model / Product DescriptionAC 309L-15 3/16X14X10#HS
Item Weight10.00
Min Order10
Filler Metal Spec Def 
Size3/16
Length14 in.
Weight10 lbs.
PackageHermetically Sealed Can