ARCALOY 309MoL-15

Arcaloy 309MoL-15 is designed for applications requiring molybdenum with a standard 309L analysis. Ideal for cladding prior to joining stainless steel to low alloy steels. Best used out-of-position on DC current.

Ordering Information
SKU251095584
UPC 
Model / Product DescriptionAC 309LMO-15 3/32X12X10#HS SPECIAL ORDER ONLY
Item Weight0.00
Min Order10
Filler Metal Spec Def 
PackageHermetically Sealed Can