ARCALOY 309/309H-15

Arcaloy 309/309H-15 is used for welding type 309 when high temperature service is required. Best used out-of-position on DC current.

Ordering Information
SKU251055976
UPC662303040987
Model / Product DescriptionAC 309/309H-15 5/32X14X10#HS
Item Weight10.00
Min Order10
Filler Metal Spec Def 
Size5/32 , 14
Length14 in., 10 in.
Weight10 lbs., Hermetically Sealed Can lbs.
PackageHermetically Sealed Can