Print this page

Arcaloy 310-16

Arcaloy 310-16 electrodes were developed for the welding of type 310 stainless steel. Usable on AC or DC current.

Ordering Information
SKU251105300
UPC662303013714
Model / Product DescriptionAC 310-16 5/32X14X10#HS
Item Weight10.00
Min Order10
Filler Metal Spec Def 
Size14 , 5/32
Length10 in., 14 in.
Weight10 lbs., Hermetically Sealed Can lbs.
PackageHermetically Sealed Can

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.