Cryoarc 316L-15 is a covered electrode designed for low temperature cryogenic applications. Pre-test lot controlled formulation to maximize mechanical properties. Best used out-of-position on DC current.
| SKU | 257171801 |
|---|---|
| UPC | 662303015718 |
| Model / Product Description | CRYOARC 316L-15 1/8X14X10#HS |
| Item Weight | 10.00 |
| Min Order | 10 |
| Filler Metal Spec Def | |
| Size | 1/8 , 14 |
| Length | 14 in., 10 in. |
| Weight | 10 lbs., Hermetically Sealed Can lbs. |
| Package | Hermetically Sealed Can |
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.