OK 92.55

OK 92.55 is designed to weld 9% nickel steels giving an optimum strength and toughness combination down to 320°F (-196°C).

Ordering Information
SKU92554030G0
UPC662303080662
Model / Product DescriptionES OK92.55 4.0X350X13.2KG VP
Item Weight0.00
Min Order29
Filler Metal Spec Def 
Size5/32 , 12
Length12 in., 0 in.
Weight0 lbs., Vacuum Packed lbs.
PackageVacuum Packed