Wear-Arc 4-IP is a covered electrode hardsurfacing alloy for metal to metal wear and moderate impact and abrasion.
| SKU | 259021400 |
|---|---|
| UPC | 662303019808 |
| Model / Product Description | WA 4-IP 1/4X18X10#HS |
| Item Weight | 10.00 |
| Min Order | 10 |
| Size | 1/4 |
| Length | 18 in. |
| Weight | 10 lbs. |
| Package | Hermetically Sealed Can |