Arcaloy ER308LSi is a silicon enhanced MIG wire which significantly increases wetting action, resulting in a smooth weld to improve weldability and performance on 304 steels.
| SKU | 258123157 |
|---|---|
| UPC | 662303523589 |
| Model / Product Description | AB ER308LSI 035X250#OMP 2/PLT |
| List Price | $ 9.411 |
| Item Weight | 250.00 |
| Min Order | 500 |
| Filler Metal Spec Def | |
| Size | .035 |
| Length | 250 in. |
| Weight | 250 lbs., Octagon Marathon Pack lbs. |
| Package | Octagon Marathon Pack |
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.