Print this page

ARCALOY ER308L

Arcaloy ER308L is a low carbon grade of 308 designed for MIG or TIG of stainless steels such as AISI 301, 304, 304L steels.

Ordering Information
SKU259601243
UPC662303521936
Model / Product DescriptionAB ER308L 3/32X18X10#CT F1
List Price$ 12.595
Item Weight10.00
Min Order10
Filler Metal Spec Def 
Size3/32
Length18 in.
Weight10 lbs.
PackageCarton