Print this page

ARCALOY ER308/308H

Arcaloy ER308/308H is a high carbon grade of 308 for higher temperature requirements.

Ordering Information
SKU257015826
UPC662303034955
Model / Product DescriptionAB ER308/308H 035X33#BAWS
List Price$ 8.334
Item Weight33.00
Min Order33
Filler Metal Spec Def 
Size.035
Length33 in.
Weight33 lbs., Spool lbs.
PackageSpool

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.