ARCALOY ER309LSi

Arcaloy ER309LSi is a silicon enhanced grade of 309 which improves the welding properties such as wetting. Arcaloy ER309LSi has good general corrosion resistance.

Ordering Information
SKU258026962
UPC662303041106
Model / Product DescriptionAB ER309LSI 035X10#PSP/60CT
List Price$ 13.421
Item Weight10.00
Min Order10
Filler Metal Spec Def 
Size.035
Weight10 lbs.
PackageSpool