Arcaloy ER309LSi is a silicon enhanced grade of 309 which improves the welding properties such as wetting. Arcaloy ER309LSi has good general corrosion resistance.
| SKU | 258027010 |
|---|---|
| UPC | 662303027612 |
| Model / Product Description | AB ER309LSI 035X33#BAWS |
| List Price | $ 10.107 |
| Item Weight | 33.00 |
| Min Order | 33 |
| Filler Metal Spec Def | |
| Size | .035 |
| Length | 33 in. |
| Weight | 33 lbs., Spool lbs. |
| Package | Spool |
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.