ARCALOY ER310

Arcaloy ER310 is used to weld stainless steel of similar composition.

Ordering Information
SKU256071945
UPC662303049126
Model / Product DescriptionAB ER310 3/32X36X10T/30#CT INK
List Price$ 13.536
Item Weight10.00
Min Order30
Filler Metal Spec Def 
Size3/32 , 36
Length36 in., 10 in.
Weight10 lbs., Tube lbs.
PackageTube