Print this page

ARCALOY ER310

Arcaloy ER310 is used to weld stainless steel of similar composition.

Ordering Information
SKU256071952
UPC662393012086
Model / Product DescriptionAB ER310 1/8X36X10T/30CT INK
List Price$ 13.329
Item Weight10.00
Min Order30
Filler Metal Spec Def 
Size1/8 , 36
Length36 in., 10 in.
Weight10 lbs., Tube lbs.
PackageTube