ARCALOY ER347

Arcaloy ER347 is a columbium stabilized stainless steel for welding types 347and 321 stainless, come in MIG, TIG, and SAW forms. Can be used in combination with OK Flux 10.93, 10.94, and/or 10.95.

Ordering Information
SKU258091115
UPC662303027919
Model / Product DescriptionAB ER347 1/16X33#PSP
List Price$ 9.042
Item Weight33.00
Min Order33
Filler Metal Spec Def 
Size1/16
Weight33 lbs.
PackageSpool

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.