Arcaloy ER410 is used to weld stainless steel of similar analysis.
| SKU | 256196312 |
|---|---|
| UPC | 662303070755 |
| Model / Product Description | AB ER410 045X30#PSP |
| List Price | $ 8.098 |
| Item Weight | 30.00 |
| Min Order | 30 |
| Filler Metal Spec Def | |
| Size | .045 |
| Weight | 30 lbs. |
| Package | Spool |