SPOOLARC 65

Spoolarc 65 is a triple deoxidize (Aluminum, Titanium, Zirconium) GMAW/GTAW welding wire. It's sluggish puddle makes it suitable for out of position welding. Spoolarc 65 produces extremely good impact properties using the GTAW process.

Ordering Information
SKU1048F05
UPC662303500863
Model / Product Description65 035X33#SP
Item Weight33.00
Min Order33
Filler Metal Spec Def 
Size.035
Length33 in.
Weight33 lbs., Spool lbs.
PackageSpool