SPOOLARC 82

Spoolarc 82 is a premium quality wire suitable for many general purpose carbon steel MIG welding applications. Spoolarc 82 is suitable for use over light rust.

Ordering Information
SKU1212F85
UPC662303504342
Model / Product Description82 035X2#SP RANDOM WOUND
Item Weight2.00
Min Order60
Filler Metal Spec Def 
Size.035
Length2 in.
Weight2 lbs., Spool lbs.
PackageSpool