SPOOLARC 82

Spoolarc 82 is a premium quality wire suitable for many general purpose carbon steel MIG welding applications. Spoolarc 82 is suitable for use over light rust.

Ordering Information
SKU1212F87
UPC662303504359
Model / Product Description82 045X2#SP RANDOM WOUND
Item Weight2.00
Min Order2
Size.045
Weight2 lbs.
PackageSpool