SPOOLARC 82

Spoolarc 82 is a premium quality wire suitable for many general purpose carbon steel MIG welding applications. Spoolarc 82 is suitable for use over light rust.

Ordering Information
SKU1218F45
UPC662303504731
Model / Product Description82 035X60#SP
Item Weight60.00
Min Order60
Size.035
Weight60 lbs.
PackageSpool