SPOOLARC 82

Spoolarc 82 is a premium quality wire suitable for many general purpose carbon steel MIG welding applications. Spoolarc 82 is suitable for use over light rust.

Ordering Information
SKU1219F45
UPC662303516123
Model / Product Description82 035X900#MP PB PLT
Item Weight900.00
Min Order1800
Size.035
Weight1800 lbs.