SPOOLARC 82

Spoolarc 82 is a premium quality wire suitable for many general purpose carbon steel MIG welding applications. Spoolarc 82 is suitable for use over light rust.

Ordering Information
SKU121EFDDBI
UPC662303523541
Model / Product Description82 045X35#SP MIL BATH
Item Weight35.00
Min Order35
Filler Metal Spec Def 
Size.045
Weight35 lbs.
PackageSpool