Print this page

SPOOLARC 85

Spoolarc 85 contains moderate levels of deoxidizers and is suitable for many general purpose carbon steel MIG applications. Spoolarc 85 can be used over light rust or light mill scale.

Ordering Information
SKU137UF47
UPC662303667689
Model / Product Description85 045X900#OMP 2/PLT
Item Weight900.00
Min Order1800
Filler Metal Spec Def 
Size.045
Length900 in.
Weight900 lbs., Octagon Marathon Pack lbs.
PackageOctagon Marathon Pack