Print this page

SPOOLARC 87HP

Spoolarc 87 HP features an optimized manganese to silicon ratio. It is suitable for welding over moderate amounts of rust and scale.

Ordering Information
SKU1455F65
UPC662303520137
Model / Product Description87HP 035X1000#WFRL 80-100 5 A
Item Weight1,000.00
Min Order1000
Size.035
Weight1000 lbs.

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.