Print this page

SPOOLARC 87HP

Spoolarc 87 HP features an optimized manganese to silicon ratio. It is suitable for welding over moderate amounts of rust and scale.

Ordering Information
SKU1457F08
UPC662303509019
Model / Product Description87HP 1/16X36X25#CT F1
Item Weight25.00
Min Order25
Filler Metal Spec Def 
Size1/16 , 36
Length36 in., 25 in.
Weight25 lbs., Carton lbs.
PackageCarton

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.