SPOOLARC 87HP

Spoolarc 87 HP features an optimized manganese to silicon ratio. It is suitable for welding over moderate amounts of rust and scale.

Ordering Information
SKU1458F24
UPC662303509088
Model / Product Description87HP 030X12#SPX48#CT
Item Weight12.00
Min Order12
Size.030
Weight12 lbs.