Spoolarc 81 is a medium manganese and silicon wire with nominal rust and mill scale tolerance. Typical applications include structural steels, medium strength pressure vessels, ship, barge, and offshore oil rig fabrication.
| SKU | 120UF48 |
|---|---|
| UPC | 662303668860 |
| Model / Product Description | 81 1/16X900#OMP 2/PLT |
| Item Weight | 900.00 |
| Min Order | 1800 |
| Filler Metal Spec Def | |
| Size | 1/16 |
| Length | 900 in. |
| Weight | 900 lbs., Octagon Marathon Pack lbs. |
| Package | Octagon Marathon Pack |