Spoolarc 81

Spoolarc 81 is a medium manganese and silicon wire with nominal rust and mill scale tolerance. Typical applications include structural steels, medium strength pressure vessels, ship, barge, and offshore oil rig fabrication.

Ordering Information
SKU1206F55
UPC662303503918
Model / Product Description81 3/16X700#DR
Item Weight700.00
Min Order700
Size3/16
Weight700 lbs.