ER90S-B9 is a solid wire for MIG and TIG welding of creep resisting, modified 9 percent chromium steels, such as ASTM A335 Grade P91 or ASTM A213 T91.
| SKU | 259967370 |
|---|---|
| UPC | 662303069407 |
| Model / Product Description | AUT90SB9 035X33#PSP |
| Item Weight | 33.00 |
| Min Order | 33 |
| Filler Metal Spec Def | |
| Size | .035 |
| Length | 33 in. |
| Weight | 33 lbs., Spool lbs. |
| Package | Spool |