Print this page

Autrod ER90S-B9

ER90S-B9 is a solid wire for MIG and TIG welding of creep resisting, modified 9 percent chromium steels, such as ASTM A335 Grade P91 or ASTM A213 T91.

Ordering Information
SKU259967396
UPC662303076801
Model / Product DescriptionAUT90SB9 3/32X55#CL
Item Weight55.00
Min Order55
Size3/32
Weight55 lbs.
PackageCoil

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.