SPOOLARC 83

Spoolarc 83 contains 0.5% Mo to provide higher deposit strength in both the as-welded and stress-relieved conditions. Spoolarc 83 is typically used on heavy equipment and high strength piping.

Ordering Information
SKU1267F30
UPC662303505998
Model / Product Description83 3/32X36X20#CT F2
Item Weight20.00
Min Order20
Filler Metal Spec Def 
Size3/32 , 36
Length36 in., 20 in.
Weight20 lbs., Carton lbs.
PackageCarton