SPOOLARC 83

Spoolarc 83 contains 0.5% Mo to provide higher deposit strength in both the as-welded and stress-relieved conditions. Spoolarc 83 is typically used on heavy equipment and high strength piping.

Ordering Information
SKU1269F07
UPC662303506193
Model / Product Description83 045X600#MP
Item Weight600.00
Min Order1200
Size.045
Weight1200 lbs.
PackageMarathon Pack