SPOOLARC 83

Spoolarc 83 contains 0.5% Mo to provide higher deposit strength in both the as-welded and stress-relieved conditions. Spoolarc 83 is typically used on heavy equipment and high strength piping.

Ordering Information
SKU126UF65
UPC662303668198
Model / Product Description83 035X550#OMP 20 2/PLT
Item Weight550.00
Min Order1100
Filler Metal Spec Def 
Size.035
Length550 in.
Weight550 lbs., Octagon Marathon Pack lbs.
PackageOctagon Marathon Pack