Print this page

SPOOLARC 40B

Spoolarc 40B is a 1/2% Mo containing submerged arc wire most commonly used for stress relief applications.

Ordering Information
SKU1184F35
UPC662303503062
Model / Product Description40-B 3/16X65#CL
Item Weight65.00
Min Order65
Filler Metal Spec Def 
Size3/16
Length65 in.
Weight65 lbs., Coil lbs.
PackageCoil