COREWELD 70

Coreweld 70 is a tubular wire containing ingredients primarily comprised of metal powder with additional arc stabilizers and alloying elements. The result is a high efficiency wire.

Ordering Information
SKU243410156
UPC662303076993
Model / Product DescriptionCW 70 1/16X600#OMP
Item Weight600.00
Min Order1200
Filler Metal Spec Def 
Size1/16
Length600 in.
Weight600 lbs., Octagon Marathon Pack lbs.
PackageOctagon Marathon Pack